The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 30, 2015

Filed:

Dec. 07, 2012
Applicant:

Nippon Light Metal Company, Ltd., Tokyo, JP;

Inventors:

Kaoru Sugita, Shizuoka, JP;

Yuji Ota, Shizuoka, JP;

Yoshihiro Taguchi, Shizuoka, JP;

Satoshi Takeda, Shizuoka, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22B 3/00 (2006.01); C22B 3/44 (2006.01); C22B 59/00 (2006.01); C22B 3/10 (2006.01); C22B 3/06 (2006.01); C22B 3/38 (2006.01); B09B 3/00 (2006.01);
U.S. Cl.
CPC ...
C22B 59/00 (2013.01); C22B 3/06 (2013.01); C22B 3/065 (2013.01); C22B 3/10 (2013.01); C22B 3/0067 (2013.01); B09B 3/0016 (2013.01);
Abstract

Provided is a method of recovering rare-earth elements, including causing rare-earth elements particularly including Nd and Dy to leach efficiently from a raw material for leaching which contains the rare-earth elements, and separating and recovering the rare-earth elements. The method of recovering rare-earth elements includes: a leaching step including performing leaching treatment of rare-earth elements in which an acidic slurry of a raw material for leaching which contains the rare-earth elements is held under a predetermined condition, and then subjecting the slurry obtained after the leaching treatment to solid-liquid separation, yielding a leachate containing the rare-earth elements; and a separation step of separating and recovering the rare-earth elements from the yielded leachate, in which: the raw material for leaching contains Ca as CaO at a ratio of 4 to 15 mass % and Ti as TiOat a ratio of 2 to 13 mass % in a solid component (S); an acid aqueous solution is an acid aqueous solution of hydrochloric acid and/or nitric acid; and the leaching treatment performed in the leaching step is digestion or maceration which is performed under the heating and pressurizing conditions of a temperature of 160 to 300° C. and a pressure of 0.65 to 10 MPa, and the rare-earth elements are caused to leach together with Ca in the leaching step.


Find Patent Forward Citations