The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 23, 2015

Filed:

Jun. 21, 2011
Applicants:

Hiroyuki Seki, Tokyo, JP;

Masanori Yoshida, Tokyo, JP;

Shogo Tagawa, Kitakyushu, JP;

Tomoyasu Kagawa, Kitakyushu, JP;

Inventors:

Hiroyuki Seki, Tokyo, JP;

Masanori Yoshida, Tokyo, JP;

Shogo Tagawa, Kitakyushu, JP;

Tomoyasu Kagawa, Kitakyushu, JP;

Assignees:

JX Nippon Oil & Energy Corporation, Chiyoda-ku, Tokyo, JP;

JGC Catalysts and Chemicals Ltd., Kawasaki-shi, Kanagawa, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 27/051 (2006.01); B01J 21/12 (2006.01); B01J 23/882 (2006.01); B01J 27/19 (2006.01); B01J 35/00 (2006.01); B01J 37/00 (2006.01); B01J 37/02 (2006.01); B01J 37/20 (2006.01); C10G 45/08 (2006.01); B01J 27/047 (2006.01); B01J 21/02 (2006.01); B01J 21/04 (2006.01); B01J 21/06 (2006.01);
U.S. Cl.
CPC ...
B01J 27/051 (2013.01); B01J 21/063 (2013.01); B01J 21/12 (2013.01); B01J 23/882 (2013.01); B01J 27/19 (2013.01); B01J 35/0013 (2013.01); B01J 37/0045 (2013.01); B01J 37/0203 (2013.01); B01J 37/20 (2013.01); C10G 45/08 (2013.01); C10G 2300/4018 (2013.01); C10G 2300/1059 (2013.01); C10G 2300/1074 (2013.01); C10G 2300/202 (2013.01); C10G 2300/207 (2013.01);
Abstract

A hydrodesulfurization catalyst is produced by pre-sulfurizing a hydrodesulfurization catalyst Y including a support containing silica, alumina and titania and at least one metal component supported thereon and selected from VIA and VIII groups of the periodic table (comprising at least Mo), in which the total area of the diffraction peak area indicating the crystal structure of anatase titania (101) planes and the diffraction peak area indicating the crystal structure of rutile titania (110) planes in the support, measured by X-ray diffraction analysis being ¼ or less of the alumina diffraction peak area assigned to γ-alumina (400) planes. The molybdenum is formed into molybdenum disulfide crystal disposed in layers on the support by the pre-sulfurization, and having an average length of longer than 3.5 nm and 7 nm or shorter in the plane direction and an average number of laminated layers of more than 1.0 and 1.9 or fewer.