The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 26, 2015

Filed:

Oct. 27, 2008
Applicants:

Klaus Bernreitner, Linz, AT;

Tung Pham, Linz, AT;

Jens Reussner, Eidenberg, AT;

Inventors:

Klaus Bernreitner, Linz, AT;

Tung Pham, Linz, AT;

Jens Reussner, Eidenberg, AT;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 23/00 (2006.01); C08L 23/08 (2006.01); C08L 9/00 (2006.01); C08L 23/10 (2006.01); C08L 23/12 (2006.01); C08L 23/14 (2006.01);
U.S. Cl.
CPC ...
C08L 23/0815 (2013.01); C08L 9/00 (2013.01); C08L 23/0807 (2013.01); C08L 23/10 (2013.01); C08L 23/12 (2013.01); C08L 23/142 (2013.01);
Abstract

The present invention relates to a polymer composition, comprising: (i) a polypropylene matrix; (ii) a first elastomeric phase dispersed within the matrix and having a glass transition temperature Tg1, measured with dynamical mechanical thermal analysis according to ISO 6721-2, wherein the first elastomeric phase comprises an ethylene copolymer having comonomer units derived from Cto Colefins; (iii) a second elastomeric phase dispersed within the matrix, wherein the second elastomeric phase is crosslinked and has a glass transition temperature Tg2, measured with dynamical mechanical thermal analysis according to ISO 6721-2, within the range of −70° C. to −90° C., wherein the difference between Tg1 and Tg2 is at least 15° C. and Tg1 is higher than Tg2.


Find Patent Forward Citations

Loading…