The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 19, 2015

Filed:

Mar. 13, 2012
Applicant:

Vladimir Ronin, Luleå, SE;

Inventor:

Vladimir Ronin, Luleå, SE;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B02B 5/02 (2006.01); B02C 19/00 (2006.01); B02C 17/00 (2006.01); B02C 17/02 (2006.01); B02C 7/00 (2006.01); C04B 7/00 (2006.01); C04B 14/00 (2006.01); C04B 7/52 (2006.01); C04B 7/13 (2006.01); C04B 14/06 (2006.01); C04B 14/08 (2006.01); C04B 14/14 (2006.01); C04B 18/08 (2006.01); C04B 20/00 (2006.01); C04B 20/02 (2006.01); C04B 28/04 (2006.01);
U.S. Cl.
CPC ...
C04B 7/13 (2013.01); C04B 14/06 (2013.01); C04B 14/08 (2013.01); C04B 14/14 (2013.01); C04B 18/08 (2013.01); C04B 20/008 (2013.01); C04B 20/026 (2013.01); C04B 28/04 (2013.01);
Abstract

The method includes subjecting the pozzolans in crushed state to a high energetic mechanical processing by grinding in a grinding equipment, whereby the pozzolan particles receive mechanical impulses, and the grinding is carried out for a predetermined time resulting in a compressive strength of a 2 inch side cube of mortar having 80% Portland cement and 20% natural pozzolan in a ratio of 1:2.75 to standard sand and in addition water required to obtain a flow of the mortar according to American standard ASTM C 109, which has been properly compacted under vibration and hardened at +20° C. in sealed condition, which after 28 days is ≧75% of the compressive strength of a 2 inch side cube, treated as the cube, of a mortar having a ratio of Portland cement:sand of 1:2.75 and water corresponding to 48.5% of the weight of Portland cement.