The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 05, 2015

Filed:

Oct. 01, 2008
Applicants:

Kazuhiro Yano, Osaka, JP;

Yoshinobu Takaki, Osaka, JP;

Inventors:

Kazuhiro Yano, Osaka, JP;

Yoshinobu Takaki, Osaka, JP;

Assignee:

Hitachi Zosen Corporation, Osaka-shi, JP;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B01D 71/02 (2006.01); B01D 69/04 (2006.01); B32B 37/06 (2006.01); C04B 35/14 (2006.01); B01D 65/00 (2006.01); B01D 63/06 (2006.01); B01D 69/10 (2006.01); C04B 35/117 (2006.01); C04B 37/00 (2006.01); C04B 38/00 (2006.01); C03C 8/04 (2006.01); C03C 8/24 (2006.01); C04B 111/00 (2006.01);
U.S. Cl.
CPC ...
B01D 65/003 (2013.01); B01D 63/061 (2013.01); B01D 69/10 (2013.01); B01D 71/028 (2013.01); B01D 2313/04 (2013.01); C04B 35/117 (2013.01); C04B 37/005 (2013.01); C04B 38/00 (2013.01); C04B 2111/00793 (2013.01); C04B 2235/786 (2013.01); C04B 2237/062 (2013.01); C04B 2237/10 (2013.01); C04B 2237/343 (2013.01); C04B 2237/76 (2013.01); C04B 2237/88 (2013.01); C03C 8/04 (2013.01); C03C 8/24 (2013.01);
Abstract

A separation membrane according to the present invention is characterized by having a porous tube containing an alumina as a main component and an attachment member disposed in a connection position of the porous tube, wherein the porous tube and the attachment member are bonded by a ceramic oxide-based bonding agent containing 17 to 48 wt % of SiO, 2 to 8 wt % of AlO, 24 to 60 wt % of BaO, and 0.5 to 5 wt % of ZnO as essential components and containing at least one of LaO, CaO, and SrO, and a thin zeolite layer is formed on a surface of the porous tube. The attachment member is bonded to the porous tube before the formation of the zeolite layer. Therefore, the bonding agent can have a melting temperature higher than 600° C., which is the upper heatproof temperature limit of the zeolite. Thus, the ceramic oxide material for the bonding agent can be selected from a wider range of compositions such as glass compositions (without limitations on the glass softening temperature).


Find Patent Forward Citations

Loading…