The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 28, 2015

Filed:

Feb. 07, 2012
Applicants:

Asami Takenaka, Tokyo, JP;

Shigehiro Tanaka, Tokyo, JP;

Yukari Ishibashi, Tokyo, JP;

Inventors:

Asami Takenaka, Tokyo, JP;

Shigehiro Tanaka, Tokyo, JP;

Yukari Ishibashi, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C08G 18/83 (2006.01); C08K 5/3417 (2006.01); C08K 5/3437 (2006.01); C08L 75/04 (2006.01); C08G 18/04 (2006.01); C09C 1/56 (2006.01); C09D 17/00 (2006.01); C09D 11/324 (2014.01); C08G 18/66 (2006.01); C08G 18/75 (2006.01); C08G 18/08 (2006.01); C08G 18/34 (2006.01); C08G 18/36 (2006.01); C08G 18/38 (2006.01); B82Y 30/00 (2011.01);
U.S. Cl.
CPC ...
C08G 18/833 (2013.01); C09C 1/56 (2013.01); C09D 17/001 (2013.01); C09D 11/324 (2013.01); C08G 18/6662 (2013.01); C08G 18/755 (2013.01); C08G 18/0823 (2013.01); C08G 18/348 (2013.01); C08G 18/36 (2013.01); C08G 18/3819 (2013.01); C01P 2004/62 (2013.01); C01P 2004/64 (2013.01); C01P 2006/12 (2013.01); C01P 2006/19 (2013.01); B82Y 30/00 (2013.01);
Abstract

A method for producing a pigment dispersion composition having excellent image density, dispersibility, and storage stability, has high resolubility, and forms an ink film having excellent marker resistance and scratch resistance. The method includes bringing a pigment (I) having a surface acidic group and a basic compound (II) having two or more ammo groups selected from a primary amino group and a secondary amino group in its molecule, into contact with each other in an aqueous medium to prepare a pigment having an unreacted surface amino group, bringing the pigment into contact with a polyisocyanate polyurethane resin (III) having two or more isocyanate end groups so that the pigment and the polyisocyanate polyurethane resin are bonded via a urea bond to prepare a dispersion of a polyurethane resin-bonded pigment (A), and heating the dispersion of the polyurethane resin-bonded pigment (A) at 40 to 100° C. for 1 to 30 days.