The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 21, 2015

Filed:

Oct. 05, 2006
Applicants:

Hiroaki Otsuka, Futtsu, JP;

Hideki Fujii, Futtsu, JP;

Kiyonori Tokuno, Tokyo, JP;

Yoshiaki Itami, Futtsu, JP;

Takashi Domoto, Tokyo, JP;

Inventors:

Hiroaki Otsuka, Futtsu, JP;

Hideki Fujii, Futtsu, JP;

Kiyonori Tokuno, Tokyo, JP;

Yoshiaki Itami, Futtsu, JP;

Takashi Domoto, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B05D 1/12 (2006.01); C22C 14/00 (2006.01); C09D 5/10 (2006.01); C09D 5/18 (2006.01); C22F 1/18 (2006.01); F01N 13/16 (2010.01); C23C 26/00 (2006.01);
U.S. Cl.
CPC ...
C22C 14/00 (2013.01); C09D 5/103 (2013.01); C09D 5/18 (2013.01); C22F 1/183 (2013.01); F01N 13/16 (2013.01); C23C 26/00 (2013.01);
Abstract

The present invention provides a titanium sheet covered with a protective film superior in high temperature oxidation resistance and high temperature salt damage resistance and a method of production of the same and an automobile exhaust system using the same. The titanium sheet covered with a protective film is formed on its surface with a protective film of a thickness of 1 to 100 μm where flake-shaped metal Al with an average thickness of 0.1 to 5 μm and average width or average length of 1 to 50 μm or grain-shaped metal Al with an average size of 0.1 to 30 μm is dispersed in 20 to 60 mass % silicone resin or silicone grease and comprised of Si: 15 to 55 mass % and C: 10 to 45 mass % and having a balance of unavoidable impurities. Preferably the titanium sheet of the substrate contains one or both of 0.5 to 2.1 mass % of Cu and 0.4 to 2.5 mass % of Al. The method of production is to brush or spray the above composition of a silicone resin on a titanium sheet to form a protective film and heat it at 150 to 300° C. for 5 to 60 minutes.