The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 21, 2015

Filed:

Jan. 28, 2009
Applicants:

Tatsuya Nakagaito, Fukuyama, JP;

Saiji Matsuoka, Kurashiki, JP;

Yoshitsugu Suzuki, Fukuyama, JP;

Yuki Toji, Fukuyama, JP;

Inventors:

Tatsuya Nakagaito, Fukuyama, JP;

Saiji Matsuoka, Kurashiki, JP;

Yoshitsugu Suzuki, Fukuyama, JP;

Yuki Toji, Fukuyama, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/00 (2006.01); C22C 38/08 (2006.01); C22C 38/18 (2006.01); C23C 2/02 (2006.01); C22C 38/02 (2006.01); C21D 1/25 (2006.01); C21D 6/00 (2006.01); C21D 8/04 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01);
U.S. Cl.
CPC ...
C22C 38/02 (2013.01); C21D 1/25 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0426 (2013.01); C21D 8/0436 (2013.01); C21D 8/0463 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01);
Abstract

A high-strength galvanized steel sheet has excellent mechanical properties such as a TS of 1200 MPa or more, an El of 13% or more, and a hole expansion ratio of 50% or more and a method for manufacturing the same. A high-strength galvanized steel sheet excellent in formability contains 0.05% to 0.5% C, 0.01% to 2.5% Si, 0.5% to 3.5% Mn, 0.003% to 0.100% P, 0.02% or less S, and 0.010% to 0.5% Al on a mass basis, the remainder being Fe and unavoidable impurities, and has a microstructure which contains 0% to 10% ferrite, 0% to 10% martensite, and 60% to 95% tempered martensite on an area basis as determined by structure observation and which further contains 5% to 20% retained austenite as determined by X-ray diffractometry.