The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 07, 2015

Filed:

Apr. 15, 2011
Applicants:

Takahide Kudoh, Iwaki, JP;

Naohiro Kagawa, Iwaki, JP;

Takashi Umemura, Iwaki, JP;

Inventors:

Takahide Kudoh, Iwaki, JP;

Naohiro Kagawa, Iwaki, JP;

Takashi Umemura, Iwaki, JP;

Assignee:

Tungaloy Corporation, Iwaki-shi, Fukushima, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 41/00 (2006.01); C22C 26/00 (2006.01); C04B 35/5831 (2006.01); C04B 35/63 (2006.01); C04B 41/45 (2006.01); C04B 41/81 (2006.01); B22F 7/02 (2006.01);
U.S. Cl.
CPC ...
C22C 26/00 (2013.01); C04B 35/5831 (2013.01); C04B 35/6303 (2013.01); C04B 41/009 (2013.01); C04B 41/4529 (2013.01); C04B 41/81 (2013.01); B22F 7/02 (2013.01); C04B 2235/3217 (2013.01); C04B 2235/3804 (2013.01); C04B 2235/3813 (2013.01); C04B 2235/3843 (2013.01); C04B 2235/3847 (2013.01); C04B 2235/3852 (2013.01); C04B 2235/3856 (2013.01); C04B 2235/3865 (2013.01); C04B 2235/3886 (2013.01); C04B 2235/402 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/5445 (2013.01); C04B 2235/5472 (2013.01); C04B 2235/80 (2013.01); C04B 2235/9607 (2013.01); C22C 2026/003 (2013.01);
Abstract

A coated cBN sintered body has excellent wear resistance, fracture resistance, adhesiveness between a substrate and a coating, and a tool life of which is elongated as compared with conventional cBN sintered bodies. The coated cBN sintered body has a cBN sintered body substrate and a coating coated on the surface thereof. The cBN sintered body includes 76 to 90% by volume of cBN, and 10 to 24% by volume of a binder phase and inevitable impurities. An average grain size of cBN is 0.5 to 5.0 μm, an average value of the thickness of the binder phase is 0.05 to 0.8 μm, and the standard deviation of the thickness of the binder phase is 0.8 μm or less.