The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 17, 2015

Filed:

Jun. 15, 2012
Applicants:

Yingchao Zhang, Louisville, KY (US);

Raman C. Subrayan, Louisville, KY (US);

Vinay Malhotra, Louisville, KY (US);

David A. Snover, Floyds Knobs, IN (US);

Inventors:

Yingchao Zhang, Louisville, KY (US);

Raman C. Subrayan, Louisville, KY (US);

Vinay Malhotra, Louisville, KY (US);

David A. Snover, Floyds Knobs, IN (US);

Assignee:

Hexion Inc., Columbus, OH (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B32B 5/02 (2006.01); B32B 27/30 (2006.01); B32B 27/36 (2006.01); B32B 27/42 (2006.01); B32B 17/04 (2006.01); C03C 25/24 (2006.01); C08K 5/07 (2006.01); C08L 29/04 (2006.01); C08L 33/00 (2006.01); C08L 33/02 (2006.01); C08L 33/08 (2006.01); C08L 33/26 (2006.01); C08L 67/00 (2006.01); D04H 1/587 (2012.01); D04H 1/64 (2012.01); D04H 13/00 (2006.01); D06M 13/224 (2006.01);
U.S. Cl.
CPC ...
D04H 1/587 (2013.01); C03C 25/24 (2013.01); C08K 5/07 (2013.01); C08L 29/04 (2013.01); C08L 33/00 (2013.01); C08L 33/02 (2013.01); C08L 33/08 (2013.01); C08L 33/26 (2013.01); C08L 67/00 (2013.01); D04H 1/64 (2013.01); D04H 13/00 (2013.01); D06M 13/224 (2013.01);
Abstract

Polyester materials, methods for making polyesters materials, and uses of the polyester materials in binder materials and articles of manufacture are disclosed. In one embodiment, a process is provided for preparing a polyester solution, including mixing monomers of at least one organic acid containing at least three carboxylic groups and at least one multi-hydroxyl alcohol containing at least three hydroxyl groups to form a reaction mixture, heating the reaction mixture to a first temperature, polymerizing the monomers at the first temperature until reaching an acid value from about 200 to about 400 mg KOH/g, adjusting the temperature to a second temperature less than the first temperature, and forming the polyester solution. The polyester materials may be mixed with cross-linking materials to form binder materials. The binder material may then be used to form articles of manufacture.


Find Patent Forward Citations

Loading…