The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 24, 2015

Filed:

Jun. 15, 2012
Applicants:

Arthur Joseph Fontenot, Iii, Baton Rouge, LA (US);

John Paul Krug, Painted Post, NY (US);

Inventors:

Arthur Joseph Fontenot, III, Baton Rouge, LA (US);

John Paul Krug, Painted Post, NY (US);

Assignee:

Lion Copolymer Geismar, LLC, Geismar, LA (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C08K 5/15 (2006.01); C08K 5/00 (2006.01); C08K 5/101 (2006.01); C08K 5/1515 (2006.01); C08J 3/22 (2006.01); C08K 3/00 (2006.01);
U.S. Cl.
CPC ...
C08K 5/0008 (2013.01); C08K 5/0016 (2013.01); C08K 5/101 (2013.01); C08K 5/1515 (2013.01); C08J 3/22 (2013.01); C08J 2323/16 (2013.01); C08K 3/0033 (2013.01);
Abstract

A durable substrate coating and a process of making include a resin master batch. The resin master batch can include ethylene propylene diene with a polymethylene backbone, mineral spirits, fillers, a de-tackifier, a curative, an activator component, and a metal dryer. The process can include adding the mineral spirits to: the ethylene propylene diene, a plasticizer, and the de-tackifier, and blending to form a solution. The process can include adding the fillers, a light stabilizer, a rheology modifier, and a pigment to the solution, forming a first mixture. The process can include adding another rheology modifier, another light stabilizer, an antioxidant, and a curative to the first mixture, forming a second mixture. The process can include mixing the second mixture to homogenously disperse each ingredient while maintaining a temperature of 60 degrees Celsius to prevent the mineral spirits from flashing.