The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 24, 2015

Filed:

Mar. 28, 2011
Applicants:

Amy L. Prieto, Fort Collins, CO (US);

Derek C. Johnson, Johnstown, CO (US);

James M. Mosby, Fort Collins, CO (US);

Inventors:

Amy L. Prieto, Fort Collins, CO (US);

Derek C. Johnson, Johnstown, CO (US);

James M. Mosby, Fort Collins, CO (US);

Assignee:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B01D 59/42 (2006.01); C25D 13/02 (2006.01); H01M 4/04 (2006.01); H01M 4/1395 (2010.01); H01M 10/052 (2010.01); H01M 10/0562 (2010.01); G01N 31/16 (2006.01); C25D 3/58 (2006.01);
U.S. Cl.
CPC ...
C25D 13/02 (2013.01); H01M 4/045 (2013.01); H01M 4/1395 (2013.01); H01M 10/052 (2013.01); H01M 10/0562 (2013.01); Y02E 60/122 (2013.01); G01N 31/164 (2013.01); C25D 3/58 (2013.01);
Abstract

An apparatus and method for measuring the isoelectric pH for materials deposited on or otherwise affixed onto and in contact with an electrode surface, and a method for utilizing the isoelectric pH to form nanometer thickness, self-assembled layers on the material, are described. Forming such layers utilizing information obtained about the isoelectric pH values of the substrate and the coating is advantageous since the growth of the coating is self-limiting because once the surface charge has been neutralized there is no longer a driving force for the solid electrolyte coating thickness to increase, and uniform coatings without pinhole defects will be produced because a local driving force for assembly will exist if any bare electrode material is exposed to the solution. The present self-assembly procedure, when combined with electrodeposition, may be used to increase the coating thickness. Self-assembly, with or without additional electrodeposition, allows intimate contact between the anode, electrolyte and cathode which is required for successful application to solid-state batteries, as an example.