The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 24, 2015

Filed:

May. 25, 2012
Applicants:

Stig Åke Andersin, Robertsfors, SE;

Bernd Heinrich Ries, Huenfeld, DE;

Frank Friedrich Lachmann, Burghaun, DE;

Lars-ivar Nilsson, Robertfors, SE;

Inventors:

Stig Åke Andersin, Robertsfors, SE;

Bernd Heinrich Ries, Huenfeld, DE;

Frank Friedrich Lachmann, Burghaun, DE;

Lars-Ivar Nilsson, Robertfors, SE;

Assignee:

Element Six Limited, County Clare, IE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 37/00 (2006.01); C03B 29/00 (2006.01); C04B 35/52 (2006.01); C04B 35/56 (2006.01); C04B 35/58 (2006.01); C04B 35/581 (2006.01); C04B 35/5831 (2006.01); C04B 35/645 (2006.01); C04B 37/02 (2006.01); C22C 26/00 (2006.01); E21B 10/46 (2006.01); B24D 11/00 (2006.01); B24D 3/02 (2006.01); B22F 7/00 (2006.01); C22C 32/00 (2006.01); C21D 1/00 (2006.01); B22F 1/00 (2006.01); C22C 1/04 (2006.01); B22F 5/00 (2006.01);
U.S. Cl.
CPC ...
C04B 37/001 (2013.01); C04B 35/52 (2013.01); C04B 35/5611 (2013.01); C04B 35/58021 (2013.01); C04B 35/581 (2013.01); C04B 35/5831 (2013.01); C04B 35/645 (2013.01); C04B 37/021 (2013.01); C22C 26/00 (2013.01); E21B 10/46 (2013.01); C04B 2235/3804 (2013.01); C04B 2235/3843 (2013.01); C04B 2235/3847 (2013.01); C04B 2235/3856 (2013.01); C04B 2235/386 (2013.01); C04B 2235/3865 (2013.01); C04B 2235/3886 (2013.01); C04B 2235/402 (2013.01); C04B 2235/427 (2013.01); C04B 2235/442 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/6565 (2013.01); C04B 2235/6567 (2013.01); C04B 2235/662 (2013.01); C04B 2235/785 (2013.01); C04B 2235/786 (2013.01); C04B 2235/80 (2013.01); C04B 2237/36 (2013.01); C04B 2237/361 (2013.01); C04B 2237/366 (2013.01); C04B 2237/401 (2013.01); C04B 2237/706 (2013.01); B22F 2005/001 (2013.01);
Abstract

A method for making a treated super-hard structure, the method including providing a super-hard structure comprising super-hard material selected from polycrystalline cubic boron nitride (PCBN) material or thermally stable polycrystalline diamond (PCD) material; subjecting the super-hard structure to heat treatment at a treatment temperature of greater than 700 degrees centigrade at a treatment pressure at which the super-hard material is not thermodynamically stable, for a treatment period of at least about 5 minutes to produce the treated super-hard structure.


Find Patent Forward Citations