The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 30, 2014

Filed:

Mar. 04, 2011
Applicants:

Tetsuro Tohma, Niihama, JP;

Kentaro Iwasaki, Niihama, JP;

Inventors:

Tetsuro Tohma, Niihama, JP;

Kentaro Iwasaki, Niihama, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/00 (2006.01); C04B 38/06 (2006.01); C04B 35/478 (2006.01); C04B 35/634 (2006.01); C04B 111/00 (2006.01);
U.S. Cl.
CPC ...
C04B 38/0645 (2013.01); C04B 35/478 (2013.01); C04B 35/63488 (2013.01); C04B 2111/00793 (2013.01); C04B 2235/3206 (2013.01); C04B 2235/3217 (2013.01); C04B 2235/3218 (2013.01); C04B 2235/322 (2013.01); C04B 2235/3232 (2013.01); C04B 2235/36 (2013.01); C04B 2235/3852 (2013.01); C04B 2235/3886 (2013.01); C04B 2235/401 (2013.01); C04B 2235/402 (2013.01); C04B 2235/404 (2013.01); C04B 2235/428 (2013.01); C04B 2235/44 (2013.01); C04B 2235/441 (2013.01); C04B 2235/442 (2013.01); C04B 2235/443 (2013.01); C04B 2235/444 (2013.01); C04B 2235/446 (2013.01); C04B 2235/447 (2013.01); C04B 2235/448 (2013.01); C04B 2235/449 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/5463 (2013.01); C04B 2235/661 (2013.01); C04B 2235/79 (2013.01); C04B 2235/3418 (2013.01); C04B 2235/5445 (2013.01); C04B 2235/6584 (2013.01);
Abstract

The production method of the present invention is a method for producing porous aluminum magnesium titanate by forming a mixture containing Al source powder, Mg source powder, Ti source powder and Si source powder as well as a pore-forming agent to obtain a molded body; presintering the obtained molded body; and then sintering the presintered molded body, wherein the content of the pore-forming agent to a total of 100 parts by mass for the Al source powder, Mg source powder, Ti source powder and Si source powder is 5 to 30 parts by mass, the melting point of the Si source powder is 600 to 1300° C., when the elemental composition ratio of Al, Mg, Ti and Si in the mixture is represented by compositional formula (1):AlMgTiO+aAlO+bSiO  (1),x satisfies 0.05≦x≦0.15, a satisfies 0≦a≦0.1 and b satisfies 0.05≦b≦0.15, and the presintered molded body is sintered at 1300 to 1560° C.