The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 09, 2014

Filed:

Apr. 23, 2009
Applicants:

Thilo Mohr, Homburg, DE;

Detlef Busch, Saarlouis, DE;

Bertram Schmitz, Saargemunies, FR;

Christian Peters, St. Ingbert, DE;

Inventors:

Thilo Mohr, Homburg, DE;

Detlef Busch, Saarlouis, DE;

Bertram Schmitz, Saargemunies, FR;

Christian Peters, St. Ingbert, DE;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 2/16 (2006.01); B32B 7/02 (2006.01); B29C 55/12 (2006.01); B32B 27/32 (2006.01); C08L 23/12 (2006.01); B32B 27/18 (2006.01); B29C 55/02 (2006.01); B29C 55/14 (2006.01); B29K 23/00 (2006.01); C08L 53/00 (2006.01); C08L 23/10 (2006.01); C08L 23/16 (2006.01); B29K 105/00 (2006.01);
U.S. Cl.
CPC ...
B29C 55/023 (2013.01); B32B 27/32 (2013.01); C08L 23/12 (2013.01); B32B 27/18 (2013.01); B29K 2023/12 (2013.01); B29K 2023/0641 (2013.01); H01M 2/1653 (2013.01); C08L 53/00 (2013.01); C08L 2207/02 (2013.01); C08L 23/10 (2013.01); C08L 23/16 (2013.01); B29K 2105/0005 (2013.01); H01M 2/16 (2013.01); B29C 55/143 (2013.01); Y10S 428/91 (2013.01);
Abstract

The invention relates to a biaxially oriented microporous film composed of at least three coextruded layers encompassing an internal cut-off layer and two external layers, wherein all three layers contain a mixture of propylene homopolymer and propylene block copolymer and β-nucleation agent. The propylene block copolymer I of the external layers has a melting point exceeding 140° C. and the propylene block copolymer II of the internal layer has a melting range starting at a temperature ranging from 50 to 120° C. and the melting point of the propylene block copolymer I is greater than the melting point of the propylene block copolymer II.