The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 09, 2014

Filed:

Feb. 24, 2012
Applicants:

Edgar Gasafi, Karlsruhe, DE;

Michael Missalla, Oberusel, DE;

Inventors:

Edgar Gasafi, Karlsruhe, DE;

Michael Missalla, Oberusel, DE;

Assignee:

Outotec Oyj, Espoo, FI;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 7/13 (2006.01); C04B 14/10 (2006.01); C04B 20/04 (2006.01); C04B 28/04 (2006.01); C04B 7/52 (2006.01); C04B 7/40 (2006.01); C04B 111/00 (2006.01);
U.S. Cl.
CPC ...
C04B 7/522 (2013.01); C04B 14/10 (2013.01); C04B 2111/00017 (2013.01); C04B 7/13 (2013.01); C04B 28/04 (2013.01); C04B 20/04 (2013.01); C04B 7/40 (2013.01);
Abstract

A method for producing a clinker substitute for use in cement production includes predrying clay with an iron content >1.5 wt-% in a form of iron oxides and a kaolinite content <40 wt-% to a moisture <10 wt-%. The clay is comminuted to a grain size <2 mm. The clay is calcined by thermal treatment in a furnace at a temperature of 600 to 1000° C. The clay is thermally treated under reducing conditions at a temperature of 600 to 1000° C. so as to form a reduction product. The reduction product is intermediately cooled to a temperature <300° C. and finally cooled.