The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 11, 2014

Filed:

Jul. 07, 2011
Applicants:

Hitoshi Furuya, Tokyo, JP;

Naoki Saitoh, Tokyo, JP;

Motohiro Okushima, Tokyo, JP;

Yasunori Takahashi, Tokyo, JP;

Takehiro Inoue, Tokyo, JP;

Ryuji Uemori, Tokyo, JP;

Inventors:

Hitoshi Furuya, Tokyo, JP;

Naoki Saitoh, Tokyo, JP;

Motohiro Okushima, Tokyo, JP;

Yasunori Takahashi, Tokyo, JP;

Takehiro Inoue, Tokyo, JP;

Ryuji Uemori, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/16 (2006.01); C22C 38/14 (2006.01); C22C 38/44 (2006.01); C21D 8/02 (2006.01); C22C 38/06 (2006.01); C21D 9/14 (2006.01); C22C 38/00 (2006.01); C22C 38/40 (2006.01); C21D 6/00 (2006.01); C21D 6/04 (2006.01); C22C 38/12 (2006.01); C21D 9/08 (2006.01);
U.S. Cl.
CPC ...
C22C 38/44 (2013.01); C22C 38/04 (2013.01); C22C 38/16 (2013.01); C22C 38/14 (2013.01); C21D 8/0226 (2013.01); C22C 38/06 (2013.01); C21D 2211/001 (2013.01); C21D 9/14 (2013.01); C22C 38/002 (2013.01); C22C 38/40 (2013.01); C21D 9/08 (2013.01); C21D 6/001 (2013.01); C22C 38/001 (2013.01); C21D 6/04 (2013.01); C22C 38/02 (2013.01); C22C 38/12 (2013.01);
Abstract

A Ni-added steel plate contains, by mass %, C: 0.03% to 0.10%, Si: 0.02% to 0.40%, Mn: 0.3% to 1.2%, Ni: 5.0% to 7.5%, Cr: 0.4% to 1.5%, Mo: 0.02% to 0.4%, Al: 0.01% to 0.08%, T.O: 0.0001% to 0.0050%, P: limited to 0.0100% or less, S: limited to 0.0035% or less, and N: limited to 0.0070% or less with a remainder composed of Fe and inevitable impurities, in which a Ni segregation ratio at a position of ¼ of a plate thickness away from a plate surface in a thickness direction is 1.3 or less, a fraction of austenite after deep cooling is 2% or more, an austenite unevenness index after deep cooling is 5.0 or less, and an average equivalent circle diameter of austenite after deep cooling is 1 μm or less.


Find Patent Forward Citations

Loading…