The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 11, 2014

Filed:

Mar. 15, 2011
Applicants:

Kei Tajima, Kobe, JP;

Kiyotaka Okuda, Kobe, JP;

Takashi Marui, Kobe, JP;

Inventors:

Kei Tajima, Kobe, JP;

Kiyotaka Okuda, Kobe, JP;

Takashi Marui, Kobe, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
F16C 13/00 (2006.01); C08L 71/03 (2006.01); C08L 9/02 (2006.01); C08L 71/02 (2006.01); G03G 15/02 (2006.01); C08K 5/00 (2006.01);
U.S. Cl.
CPC ...
G03G 15/0233 (2013.01); C08L 71/03 (2013.01); C08L 9/02 (2013.01); C08G 2261/12 (2013.01); F16C 13/00 (2013.01); C08L 71/02 (2013.01); C08K 5/0025 (2013.01);
Abstract

The semiconductive roller according to the present invention includes: a roller body having an outer peripheral surface made of a semiconductive rubber composition; and an oxide film covering the outer peripheral surface of the roller body, while the semiconductive rubber composition contains a base polymer and a crosslinking component for crosslinking the base polymer, the base polymer is a mixture of a bicopolymer E containing epichlorohydrin and nitrile-butadiene rubber N, the mass ratio E/N of the bicopolymer E and the nitrile-butadiene rubber N in the mixture is 50/50 to 80/20, and the crosslinking component includes a thiourea-based crosslinking component for crosslinking the bicopolymer E and a sulfur-based vulcanizing component for vulcanizing the nitrile-butadiene rubber N.