The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 28, 2014

Filed:

Nov. 27, 2008
Applicants:

Yoshinobu Nozue, Ichihara, JP;

Naoko Ochi, Chiba, JP;

Yasutoyo Kawashima, Ichihara, JP;

Inventors:

Yoshinobu Nozue, Ichihara, JP;

Naoko Ochi, Chiba, JP;

Yasutoyo Kawashima, Ichihara, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 210/00 (2006.01); C08F 210/16 (2006.01); C08F 4/659 (2006.01); C08F 4/6592 (2006.01);
U.S. Cl.
CPC ...
C08F 210/16 (2013.01); C08F 2410/01 (2013.01); C08F 4/65912 (2013.01); C08F 4/65927 (2013.01); C08F 4/65916 (2013.01);
Abstract

An ethylene-α-olefin copolymer wherein the copolymer has a monomer unit based on ethylene and a monomer unit based on an α-olefin having 3 to 20 carbon atoms, the density (d) is 860 to 950 kg/m, the melt flow rate (MFR) is 1 to 100 g/10 min, the ratio (Mw/Mn) of the weight average molecular weight (Mw) to the number average molecular weight (Mn) is 4 to 30, the ratio (Mz/Mw) of the Z average molecular weight (Mz) to the weight average molecular weight (Mw) is 2 to 5, the swell ratio (SR) is 1.8 or more, and the characteristic relaxation time (τ) obtained by linear viscoelasticity measurement is 0.01 to 10 seconds.