The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 07, 2014

Filed:

Apr. 19, 2011
Applicants:

Yasushi Ichikawa, Tokyo, JP;

Hideharu Kimura, Tokyo, JP;

Akira Ishii, Tokyo, JP;

Inventors:

Yasushi Ichikawa, Tokyo, JP;

Hideharu Kimura, Tokyo, JP;

Akira Ishii, Tokyo, JP;

Assignee:

Showa Denko K.K., Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B01J 19/20 (2006.01); C08G 18/42 (2006.01); C08G 18/73 (2006.01); C08G 18/08 (2006.01);
U.S. Cl.
CPC ...
C08G 18/4238 (2013.01); C08G 18/73 (2013.01); C08G 18/0895 (2013.01);
Abstract

The present invention addresses the problem of providing a method for continuously and effectively producing an aliphatic polyester having an increased molecular weight by preventing evaporation of a diisocyanate when blending the diisocyanate with an aliphatic polyester prepolymer in a molten state at a temperature not lower than the melting point thereof so that the diisocyanate and the aliphatic polyester prepolymer are uniformly blended. In order to solve the above-mentioned problem, the present invention provides a method for producing an aliphatic polyester having an increased molecular weight comprising the steps of (i) quantitatively injecting a diisocyanate into an aliphatic polyester prepolymer which has a number average molecular weight of 5,000 or higher and has terminal hydroxyl groups and in which at least one acid component is a succinic acid compound, in a melting state at a temperature not lower than the melting point thereof wherein the amount of the diisocyanate is equivalent to between one tenth and two times the amount of hydroxyl groups in the aliphatic polyester prepolymer, (ii) quantitatively and continuously introducing the diisocyanate-containing aliphatic polyester prepolymer obtained at the step (i) into a mixing tank, discharging same from the mixing tank under stirring and supplying it to a coupling reaction tank, and (iii) reacting the aliphatic polyester prepolymer with the diisocyanate in the coupling reaction tank.