The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 30, 2014

Filed:

May. 14, 2010
Applicants:

Kristian Dahlen, Stora Höga, SE;

Roger Carlsson, Säve, SE;

Inventors:

Kristian Dahlen, Stora Höga, SE;

Roger Carlsson, Säve, SE;

Assignee:

Borealis AG, Vienna, AT;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08G 77/08 (2006.01); C08F 255/02 (2006.01); C08L 51/06 (2006.01); C08F 255/00 (2006.01);
U.S. Cl.
CPC ...
C08F 255/00 (2013.01); C08F 255/02 (2013.01); C08L 51/06 (2013.01);
Abstract

The present invention relates to a polyolefin composition comprising (A) a crosslinkable polyolefin with hydrolysable silane groups which upon hydrolysation form an acid or a base, characterised in that the acid or base generates a gel content of at least 40% after 40 hours in the 90° C. cross-linking test, wherein the acid or base is added in an amount of 4.5 mmol/kg to an ethylene/vinyltrimethoxysilane copolymer with a MFR=2 g/10 min, a density of 923 g/cm, and 2 wt. % of vinyltrimethoxysilane and then is cross-linked in a waterbath at 90° C., and to a polyolefin composition comprising (i) a crosslinkable polyolefin with hydrolysable silane groups, and (ii) a non-polymeric compound with hydrolysable silane groups which upon hydrolysation form an acid or a base, characterised in that the acid or base generates a gel content of at least 40% after 40 hours in the 90° C. cross-linking test, wherein the acid or base is added in an amount of 4.5 mmol/kg to an ethylene/vinyltrimethoxysilane copolymer with a MFR=2 g/10 min, a density of 923 g/cm, and 2 wt. % of vinyltrimethoxysilane and then is cross-linked in a waterbath at 90° C.


Find Patent Forward Citations

Loading…