The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 16, 2014

Filed:

Jun. 11, 2004
Applicants:

Animesh Jha, Leeds, GB;

Pailo Antony Malpan, Kalpakkam, IN;

Vilas Dattatray Tathavadkar, Phaltan, IN;

Inventors:

Animesh Jha, Leeds, GB;

Pailo Antony Malpan, Kalpakkam, IN;

Vilas Dattatray Tathavadkar, Phaltan, IN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22B 9/00 (2006.01); B22D 11/10 (2006.01); C21B 7/14 (2006.01); C21B 15/00 (2006.01); C21B 3/04 (2006.01); C22B 5/20 (2006.01); C22B 11/10 (2006.01); C21B 11/10 (2006.01); C01G 49/02 (2006.01); C01F 7/02 (2006.01); C01G 15/00 (2006.01); C01F 3/00 (2006.01); C01G 23/047 (2006.01); C01G 27/02 (2006.01); C01G 25/02 (2006.01); C01B 13/14 (2006.01); C01B 33/12 (2006.01); C01B 33/20 (2006.01); C01B 15/14 (2006.01); C01B 33/00 (2006.01); C22B 21/00 (2006.01); C22B 34/12 (2006.01); C01G 49/06 (2006.01); C22B 7/04 (2006.01); C22B 1/02 (2006.01); C01F 7/38 (2006.01); C01F 7/14 (2006.01); C22B 5/10 (2006.01);
U.S. Cl.
CPC ...
C22B 34/1236 (2013.01); C22B 21/0038 (2013.01); C22B 34/1259 (2013.01); C22B 34/1209 (2013.01); C01G 49/06 (2013.01); C01G 23/047 (2013.01); C22B 7/04 (2013.01); C22B 1/02 (2013.01); C01F 7/38 (2013.01); C01F 7/142 (2013.01); C22B 5/10 (2013.01);
Abstract

The present invention relates to a zero-waste process for extraction of alumina from different types of bauxite ores and red mud residues and of titanium dioxide from ilmenite. Iron oxide is first reduced to metallic iron above the melting point of C-saturated cast iron alloy which yields a high-C iron alloy and an Al and Ti metal oxide rich slag which is then treated with alkali carbonate to form alkali aluminates and titanates. The alkali aluminates are separated by water leaching from which the hydroxide of alumina is precipitated by bubbling C0. The residue from water leaching is treated with sulphuric acid and Ti0is precipitated via a hydrolysis route. The process recovers most of the metal values and generates only small quantities of silicious residues at pH 4-5 which can be used for soil conditioning. The present also relates to a method for selective separation of Ti0-rich oxides from titaniferrous ore/residue materials via oxidative roasting in the presence of alkali carbonate or carbonates followed by aqueous leaching of the roasted material and selective precipitation of Ti0under controlled condition below pH=4.