The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 09, 2014

Filed:

Feb. 01, 2011
Applicants:

Angelo Schütz, Rudolstadt, DE;

Stefan Reinemann, Rudolstadt, DE;

Inventors:

Angelo Schütz, Rudolstadt, DE;

Stefan Reinemann, Rudolstadt, DE;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
D02G 3/02 (2006.01); B29C 47/88 (2006.01); B32B 27/32 (2006.01); D01D 5/088 (2006.01); D01F 6/56 (2006.01); B29C 47/00 (2006.01); C09K 5/06 (2006.01); D01F 1/10 (2006.01); B29K 25/00 (2006.01); B29K 33/00 (2006.01); B29K 23/00 (2006.01); B29K 69/00 (2006.01); B29K 105/00 (2006.01);
U.S. Cl.
CPC ...
D01F 1/10 (2013.01); D01D 5/0885 (2013.01); B29K 2025/00 (2013.01); B29K 2033/12 (2013.01); B29C 2947/92447 (2013.01); B29C 47/8815 (2013.01); D01F 6/56 (2013.01); B29C 47/0021 (2013.01); B29C 2947/92152 (2013.01); B29K 2023/0633 (2013.01); B29K 2023/065 (2013.01); B29K 2069/00 (2013.01); B29C 2947/92209 (2013.01); C09K 5/063 (2013.01); B29K 2105/256 (2013.01);
Abstract

Fiber-like or film-like moldings are produced from a plastified mixture which, based on its weight, is from 60 to 10% by weight of a carrier component and from 40 to 90% by weight of a phase change material. The carrier component contains from 5 to 20% by weight of a polymer or polymer blend from the group of LDPE (low density polyethylene), HDPE (high density polyethylene), PMMA (polymethyl methacrylate), polycarbonate, or mixtures thereof, from 5 to 20% by weight of a styrene block copolymer, and from 0 to 20% by weight of one or more additives. Especially suitable phase change materials include natural and synthetic paraffins, polyethylene glycol (=polyethylene oxide), and mixtures thereof. The plasticized mixture is extruded through a spinneret or a slit die at a temperature of from 130 to 220° C. and is stretched.