The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 26, 2014

Filed:

Jul. 15, 2010
Applicants:

Masahiro Watanabe, Toyama, JP;

Satoshi Kondoh, Toyama, JP;

Koji Tsukuma, Kanagawa, JP;

Inventors:

Masahiro Watanabe, Toyama, JP;

Satoshi Kondoh, Toyama, JP;

Koji Tsukuma, Kanagawa, JP;

Assignee:

Tosoh Corporation, Yamaguchi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/486 (2006.01);
U.S. Cl.
CPC ...
C04B 35/486 (2013.01);
Abstract

The subject of the present invention relates to obtaining a zirconia sintered body having excellent in both properties of a translucency and a mechanical strength. The present invention relates to obtaining a high-strength zirconia sintered body having a translucency of an in-line transmission of 50% or more at a sample thickness of 1 mm for visible light at a wavelength of 600 nm and an average flexural strength of 300 MPa or more by subjecting a zirconia primary sintered body having an average grain size of 1 μm or less and a relative density of 92% or more and the crystal phase composed of cubic crystals only to HIP treatment at a temperature of 1,250° C. to 1,600° C. and a pressure of at least 50 MPa. The primary sintered body is obtained by maintaining a molded body of a zirconia powder containing 7 mol % to 30 mol % of yttria at 1,100° C. to 1,300° C. for at least 5 hrs or by heating the molded body at a high rate of temperature rise of 500° C./hr or more.