The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 26, 2014

Filed:

Dec. 24, 2008
Applicants:

Kunichika Kubota, Yasugi, JP;

Hideshi Nakatsu, Yasugi, JP;

Shugo Komatsubara, Higashiizumocho, JP;

Inventors:

Kunichika Kubota, Yasugi, JP;

Hideshi Nakatsu, Yasugi, JP;

Shugo Komatsubara, Higashiizumocho, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 38/08 (2006.01); C22C 38/46 (2006.01); C22C 38/12 (2006.01); C22C 38/18 (2006.01); C22C 38/00 (2006.01); C22C 38/44 (2006.01); C21D 8/02 (2006.01); C21D 8/00 (2006.01);
U.S. Cl.
CPC ...
Abstract

A cold die steel excellent in the characteristic of suppressing dimensional change, which has a chemical composition in mass %: C: 0.7% or more and less than 1.6%, Si: 0.5 to 3.0%, Mn: 0.1 to 3.0%, P: less than 0.05% including 0%, S: 0.01 to 0.12%, Cr: 7.0 to 13.0%, one or two elements selected from the group consisting of Mo and W: amounts satisfying the formula (Mo+(W/2))=0.5 to 1.7%, V: less than 0.7% including 0, Ni: 0.3 to 1.5%, Cu: 0.1 to 1.0% and Al: 0.1 to 0.7%. Preferably, the die steel satisfies the formula in mass %: Ni/Al=1 to 3.7. It is preferred that the die steel also satisfies the following formula in mass %: (Cr−4.2×C)=5 or less and (Cr−6.3×C)=1.4 or more and that it contains 0.3% or less of Nb.