The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jul. 01, 2014
Filed:
Sep. 28, 2010
Jin Sato, Ibaraki, JP;
Kouichi Takemoto, Ibaraki, JP;
Takeshi Sasaki, Osaka, JP;
Mikio Ohno, Osaka, JP;
Junji Ogura, Osaka, JP;
Jin Sato, Ibaraki, JP;
Kouichi Takemoto, Ibaraki, JP;
Takeshi Sasaki, Osaka, JP;
Mikio Ohno, Osaka, JP;
Junji Ogura, Osaka, JP;
JX Nippon Mining & Metals Corporation, Tokyo, JP;
Japan New Metals Co., Ltd., Osaka, JP;
Abstract
Provided is a method for producing a high-purity tungsten powder having a phosphorus content of less than 1 wtppm; wherein an ammonium tungstate solution containing 1 wtppm or more of phosphorus as an impurity in terms of the inclusion in tungsten is used as a starting material, this solution is neutralized with hydrochloric acid at a temperature of 50° C. or less to adjust the pH at 4 or more and less than 7 so as to precipitate ammonium paratungstate undecahydrate crystals, the resulting solution is heated to 70 to 90° C. and filtered in a high-temperature state so as to obtain ammonium paratungstate pentahydrate crystals, the obtained crystals are calcined so as to form a tungsten oxide, and the tungsten oxide is subject to hydrogen reduction so as to obtain a high-purity tungsten powder. Additionally provided is a method for producing a high-purity tungsten powder having a phosphorus content of 0.4 wtppm or less; wherein the ammonium tungstate solution is neutralized with hydrochloric acid to adjust the pH at 4 or more and 6 or less, and this solution is subject to the same procedure as described above so as to obtain a high-purity tungsten powder. Consequently, the phosphorus content can be efficiently reduced.