The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Apr. 08, 2014
Filed:
Nov. 28, 2008
Arturo Solis Herrera, Auguascalientes, MX;
Arturo Solis Herrera, Auguascalientes, MX;
Other;
Abstract
The present invention refers to a cement composition that contains dopamelanin, its precursors and/or its analogues as an additive in a maximum percentage of 30% of the cement. This additive substitutes water of the capillary nets. The mentioned cement mixture posses a water/cement relation of 0.2 to 0.4, optionally it can contain different sand and gravel proportions. This cement mixture generates strong chemical bonds, and increased scouring resistance, of at least 28% and a higher elastic resistance of the concrete, of at least 50%. Its cracking in early stages is very low or practically null. The present request also refers to the use of dopamelanin and/or its precursors and/or its analogues as an additive of the cement mixture that substitutes the capillary water proportion in the cementant mixture. Just as well the use of dopamelanin and/or its precursors and/or its analogues, in an aqueous solution, in less that 3%, as a concrete setting and curing agent, thus it significantly increases the ductility and scouring resistance of the cement mixture. This is, the novelty cement mixture improves the physicochemical and bacteriological properties of the usual concrete, being of special interest the notable increment related with compression resistance and ductility or relative displacements, suffering less damage in comparison with the mixture containing water. In a meaningful way, it also increases since early stages, the volumetric stability of the concrete, thus it intensifies its scouring resistance, which is inclusive transmitter to the metallic elements immersed in its interior, since certainly it significantly protects them from deterioration.