The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 18, 2014

Filed:

Jan. 27, 2011
Applicants:

Andrey Buryak, Linz, AT;

Albrecht Dix, Linz, AT;

Magnus Palmlof, Vastra Frolunda, SE;

Anneli Pakkanen, Vasterskog, FI;

Christian Piel, Linz, AT;

Ayodele Olutayo Fiola, Linz, AT;

Tore Dreng, Larvik, NO;

Janne Maaranen, Tuusula, FI;

Alexander Krajete, Linz, AT;

Susana Filipe, Leonding, AT;

Inventors:

Andrey Buryak, Linz, AT;

Albrecht Dix, Linz, AT;

Magnus Palmlof, Vastra Frolunda, SE;

Anneli Pakkanen, Vasterskog, FI;

Christian Piel, Linz, AT;

Ayodele Olutayo Fiola, Linz, AT;

Tore Dreng, Larvik, NO;

Janne Maaranen, Tuusula, FI;

Alexander Krajete, Linz, AT;

Susana Filipe, Leonding, AT;

Assignee:

Borealis AG, Vienna, AT;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 8/00 (2006.01); C08L 23/04 (2006.01);
U.S. Cl.
CPC ...
Abstract

A polyethylene moulding composition having a multimodal molecular weight distribution, having a density according to ISO 1183 at 23° C. in the range of 920 to 960 kg/mand an MFR190/2 according to ISO 1133 in the range of 0.05 to 10 g/10 min, said polyethylene moulding composition comprising at least three ethylene polymer fractions having distinct molecular weights: A) 15 to 50 wt % of a low molecular weight ethylene homopolymer or copolymer fraction with a weight average molecular weight Mw in the range of 15 to 40 kg/mol; B) 15 to 50 wt % of a medium molecular weight ethylene homopolymer or copolymer fraction with a weight average molecular weight Mw in the range of 70 to 200 kg/mol; and C) 15 to 50 wt % of a high molecular weight ethylene homopolymer or copolymer fraction with a weight average molecular weight Mw in the range of 220 to 400 kg/mol, provided that one of A, B and C is an ethylene homopolymer and at least one other component is an ethylene copolymer with at least one C-Ccomonomer; and wherein the composition has—a Shore D hardness measured according to ASTM D2240-05 (15 sec) of at least 56.0.