The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 08, 2013

Filed:

Jul. 25, 2007
Applicants:

Ryoji Yamada, Chigasaki, JP;

Koji Tatsumi, Chigasaki, JP;

Shogo Nakaoka, Chigasaki, JP;

Kenji Ito, Chigasaki, JP;

Kazuya Hiratsuka, Chigasaki, JP;

Inventors:

Ryoji Yamada, Chigasaki, JP;

Koji Tatsumi, Chigasaki, JP;

Shogo Nakaoka, Chigasaki, JP;

Kenji Ito, Chigasaki, JP;

Kazuya Hiratsuka, Chigasaki, JP;

Assignee:

AGC Seimi Chemical Co., Ltd., Chigasaki-shi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/13 (2010.01);
U.S. Cl.
CPC ...
Abstract

To provide a process for a lithium-containing composite oxide for a positive electrode for a lithium secondary battery, which has a large volume capacity density and high safety, and is excellent in the charge and discharge cyclic durability and low temperature characteristics. A process for producing a lithium-containing composite oxide represented by the formula LiNMOF(wherein N is at least one element selected from the group consisting of Co, Mn and Ni, M is at least one element selected from the group consisting of Al, alkaline earth metal elements and transition metal elements other than N, 0.9≦p≦1.2, 0.95≦x≦2.00, 0<y≦0.05, 1.9≦z≦4.2 and 0≦a≦0.05), which comprises firing a mixture of a lithium source, an N element source, an M element source and if necessary, a fluorine source, characterized in that an aqueous solution having an M element source dissolved therein is mixed with an N element source powder or its pulverized product to form a slurry; if necessary after being pulverized, the slurry is dried for granulation to obtain a granulated product, which is mixed with a lithium source powder and if necessary, a fluorine source powder to obtain a mixture; and the mixture is fired at from 700 to 1,100° C. in an oxygen-containing atmosphere.