The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Jun. 25, 2013
Filed:
Jun. 25, 2008
Hisayuki Nakashima, Kanagawa, JP;
Souichi Mori, Kanagawa, JP;
Satoshi Matsumoto, Kanagawa, JP;
Daiki Fujihira, Kanagawa, JP;
Hisayuki Nakashima, Kanagawa, JP;
Souichi Mori, Kanagawa, JP;
Satoshi Matsumoto, Kanagawa, JP;
Daiki Fujihira, Kanagawa, JP;
BASF Coatings Japan Ltd., , JP;
Abstract
To provide a method of forming a multi-layer paint film with which, even when applying three paint layers and baking the paint layer only once, it is possible to achieve a paint film appearance the same as that with the conventional baking twice method. [Means of Resolution] A method of forming a multi-layer paint film in which an aqueous first base-paint is painted on a base material on which an electro-deposition paint has been coated and a first base-paint layer is formed, an aqueous second base-paint is painted on said first base-paint layer as a wet-on-wet system and a second base-paint layer is formed and, moreover, a clear-paint is painted on the second base-paint layer as a wet-on-wet system and a clear-paint layer is formed and then the three paint layers are all baked at the same time which is characterized in that the aqueous first base-paint includes as essential components hydroxyl group containing non-ionic resin where ethylene oxide units and/or propylene oxide units are included in an amount of from 4 to 15 mass % in the resin and of which the resin acid value is less than 15 mgKOH/g and the hydroxyl group value is from 10 to 100 mgKOH/g, and crosslinking agent.