The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 18, 2012

Filed:

Jan. 11, 2010
Applicants:

James E. Boyle, Saratoga, CA (US);

Raanan Zehavi, Sunnyvale, CA (US);

Amnon Chalzel, Sunnyvale, CA (US);

Inventors:

James E. Boyle, Saratoga, CA (US);

Raanan Zehavi, Sunnyvale, CA (US);

Amnon Chalzel, Sunnyvale, CA (US);

Assignee:

Ferrotec (USA) Corporation, Santa Clara, CA (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B05D 3/02 (2006.01); B32B 5/16 (2006.01); B32B 9/00 (2006.01); B32B 17/06 (2006.01); B32B 9/04 (2006.01); B32B 13/04 (2006.01); G11B 11/105 (2006.01);
U.S. Cl.
CPC ...
Abstract

A method of joining two silicon members, the adhesive used for the method, and the joined product, especially a silicon tower for supporting multiple silicon wafers. A flowable adhesive is prepared comprising silicon particles of size less than 100 μm and preferably less than 100 nm and a silica bridging agent, such as a spin-on glass. Nano-silicon crystallites of about 20 nm size maybe formed by CVD. Larger particles maybe milled from virgin polysilicon. If necessary, a retardant such as a heavy, preferably water-insoluble alcohol such as terpineol is added to slow setting of the adhesive at room temperature. The mixture is applied to the joining areas. The silicon parts are assembled and annealed at a temperature sufficient to link the silica, preferably at 900° C. to 1100° C. for nano-silicon but higher for milled silicon.