The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 22, 2012

Filed:

Aug. 29, 2008
Applicants:

Benoit Koch, Hannut, BE;

Daniel Marissal, Carry le Rouet, FR;

Marc Parisel, Vilvoorde, BE;

Brent R Walworth, Sint-Niklaas, BE;

Inventors:

Benoit Koch, Hannut, BE;

Daniel Marissal, Carry le Rouet, FR;

Marc Parisel, Vilvoorde, BE;

Brent R Walworth, Sint-Niklaas, BE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 2/00 (2006.01); C08F 4/44 (2006.01); C08F 4/72 (2006.01); B01J 19/00 (2006.01); B01J 19/18 (2006.01); F01N 3/20 (2006.01);
U.S. Cl.
CPC ...
Abstract

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80 wt % of a low molecular weight (LMW) polymer is made in suspension in a second reactor in the presence of the HMW polymer, wherein the solids concentration in the second LMW reactor, defined as the mass of polymer divided by the total mass of slurry, is at least 35 wt %, most preferably between 45 wt % and 60 wt %, and/or the ratio of solids concentration in the first reactor to that in the second reactor is maintained at less than 1.0, preferably between 0.6 and 0.8, and further wherein the volume of the second reactor is at least 10%, preferably at least 30% and more preferably at least 50% greater than the volume of the first reactor.