The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 28, 2011

Filed:

Sep. 21, 2007
Applicants:

Yutaka Minami, Chiba, JP;

Masami Kanamaru, Chiba, JP;

Toyozo Fujioka, Chiba, JP;

Tomoaki Takebe, Chiba, JP;

Masao Inoue, Chiba, JP;

Inventors:

Yutaka Minami, Chiba, JP;

Masami Kanamaru, Chiba, JP;

Toyozo Fujioka, Chiba, JP;

Tomoaki Takebe, Chiba, JP;

Masao Inoue, Chiba, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 10/08 (2006.01); C08F 110/08 (2006.01); C08F 210/08 (2006.01);
U.S. Cl.
CPC ...
Abstract

A 1-butene polymer satisfying the following (1), (2) and either (3) or (3'): a process for producing the polymer; a resin modifier comprising the polymer; and a hot-melt adhesive containing the polymer. (1) The intrinsic viscosity [η] as measured in tetralin solvent at 135° C. is 0.01 to 0.5 dL/g. (2) The polymer is a crystalline resin having a melting point (Tm-D) of 0 to 100° C., the melting point being defined as the top of the peak observed on the highest-temperature side in a melting endothermic curve obtained with a differential scanning calorimeter (DSC) in a test in which a sample is held in a nitrogen atmosphere at −10° C. for 5 min and then heated at a rate of 10° C./min. (3) The stereoregularity index {(mmmm)/(mmrr+rmmr)} is 30 or lower. (3′) The mesopentad content (mmmm) determined from a nuclear magnetic resonance (NMR) spectrum is 68 to 73%.