The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Nov. 09, 2010
Filed:
Jun. 13, 2007
Takurou Endo, Inuyama, JP;
Masayuki Haruta, Inuyama, JP;
Norimi Tabota, Inuyama, JP;
Katsuhiko Nose, Inuyama, JP;
Takurou Endo, Inuyama, JP;
Masayuki Haruta, Inuyama, JP;
Norimi Tabota, Inuyama, JP;
Katsuhiko Nose, Inuyama, JP;
Toyo Boseki Kabushiki Kaisha, Osaka-shi, JP;
Abstract
In the heat-shrinkable polyester film of the present invention, the main shrinkage direction is the longitudinal direction. In addition, the hot-water heat shrinkage ratios in the longitudinal direction and the width direction when the film is treated in hot water at 90° C. for 10 seconds, the refractive indexes in the longitudinal direction and the width direction and the natural shrinkage ratio after aging at 40° C. and 65% RH for 700 hours or more are each controlled in predetermined ranges. The heat-shrinkable polyester film of the present invention is manufactured by stretching an unstretched film at a ratio of 2.5 times or more and 6.0 times or less in the width direction at a temperature of Tg+5° C. or more and Tg+40° C. or less, passing the film in an intermediate zone that does not execute an active heating operation, heat-treating the film at a temperature of 100° C. or more and 170° C. or less over a period of 1.0 second or more and 10.0 seconds or less, cooling the film to a surface temperature of 30° C. or more and 70° C. or less, stretching the film at a ratio of 2.0 times or more and 7 times or less in the longitudinal direction at a temperature of Tg+5° C. or more and Tg+80° C. or less, and subsequently cooling the film at a cooling rate of 30° C./second or more and 70° C./second or less to a surface temperature of the film of 45° C. or more and 75° C. or less.