The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Sep. 01, 2009
Filed:
Mar. 07, 2005
Daocheng Pan, Changchun, CN;
Shichun Jiang, Changchun, CN;
Lijia an, Changchun, CN;
Bingzheng Jiang, Changchun, CN;
Xiangling Ji, Changchun, CN;
Daocheng Pan, Changchun, CN;
Shichun Jiang, Changchun, CN;
Lijia An, Changchun, CN;
Bingzheng Jiang, Changchun, CN;
Xiangling Ji, Changchun, CN;
Abstract
The present invention provides a process for producing a nanosemiconductor luminous material on a liquid-liquid interface, comprising the steps of: a) an oxide of a Group IIB metal and a carboxylic acid with 2-18 carbon atoms or an oleic acid reacting with each other in a solvent at 150-300° C. for 5-30 min, wherein the mol ratio of the oxide to the acid being 1˜5:5˜1; b) adding trioctylphosphine oxide and trioctylphosphine with a mol ratio of trioctylphosphine oxide to trioctylphosphine of 10˜1:1˜10 and a mol ratio of the total mol numbers of trioctylphosphine oxide to the oxide of 10˜1:1˜10; c) adding an aqueous solution of at least one alkaline/alkaline earth metal chalcogenide in a mol ratio of the chalcogenide to the oxide of 10˜1:1˜10; and d) reacting at 20-100° C. for 0.5˜10 h to obtain a sol containing a semiconductor nanoparticle. The produced semiconductor nanoparticle can emit a wavelength-adjustable visible light under a UV lamp.