The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Dec. 16, 2008
Filed:
May. 12, 2004
Tadao Yoshikawa, Kurashiki, JP;
Tatsuya Sunamoto, Kurashiki, JP;
Tadao Yoshikawa, Kurashiki, JP;
Tatsuya Sunamoto, Kurashiki, JP;
Kuraray Co., Ltd., Kurashiki-shi, JP;
Abstract
The method of manufacturing a film of thermotropic liquid crystal polymer includes extruding a thermotropic liquid crystal polymer of a kind in which any one of activation energies Ea1 and Ea2 of a melt viscosity is within the range of 30 to 90 kcal/mol, with the ratio (Ea1/Ea2) of the activation energy Ea1 relative to the activation energy Ea2 being within the range of 1 to 1.7. The activation energies Ea1 and Ea2 are measured by means of a capillary rheometer, including a nozzle of 1 mm in inner diameter and 10 mm in length disposed at an angle of introduction of 90° and a barrel of 9.55 mm in inner diameter, at respective shear rates of 243 secondsand 2432 secondsunder a temperature ranging from the temperature [(Tm−10)° C.], which is lower by 10° C. than the melting point [(Tm)° C.] of the thermotropic liquid crystal polymer, to the temperature [(Tm+20)° C.], which is higher by 20° C. than the melting point [(Tm)° C.] of the thermotropic liquid crystal polymer. The thermotropic liquid crystal polymer also has a melt viscosity of not lower than 400 poises measured under predetermined conditions, and is extruded from a die that is heated to a temperature of predetermined range.