The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 07, 2006

Filed:

Sep. 17, 2004
Applicants:

Hiroyuki Kado, Osaka, JP;

Mitsuhiro Ohtani, Sakai, JP;

Masaki Aoki, Mino, JP;

Kanako Miyashita, Moriguchi, JP;

Inventors:

Hiroyuki Kado, Osaka, JP;

Mitsuhiro Ohtani, Sakai, JP;

Masaki Aoki, Mino, JP;

Kanako Miyashita, Moriguchi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01J 9/44 (2006.01);
U.S. Cl.
CPC ...
Abstract

A PDP with superior light-emitting characteristics and color reproduction is achieved by setting the chromaticity coordinate y (the CIE color specification) of light to 0.08 or less, more preferably to 0.07 or less, or 0.06 or less, enabling the color temperature of light to be set to 7,000K or more, and further to 8,000K or more, 9,000K or more, or 10,000K or more. The PDP is manufactured by a method in which the processes for heating the fluorescent substances such as the fluorescent substance baking, sealing material temporary baking, bonding, and exhausting processes are performed in the dry gas atmosphere, or in an atmosphere in which a dry gas is circulated at a pressure lower than the atmospheric pressure. This PDP is also manufactured by: a method in which after the front and back panels are bonded together, the exhausting process for exhausting gas from the inner space between panels is started while the panels are not cooled to room temperature; or a method in which after the front and back panels are temporarily baked, the process for bonding the panels is started while the panels are not cooled to room temperature. This reduces the time and energy required for heating, resulting in reduction of manufacturing cost.