The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 17, 2006

Filed:

Jul. 28, 2003
Applicants:

Michael Musgrave, Houston, TX (US);

Likuo Sun, Houston, TX (US);

Mark Miller, Houston, TX (US);

Inventors:

Michael Musgrave, Houston, TX (US);

Likuo Sun, Houston, TX (US);

Mark Miller, Houston, TX (US);

Assignee:

Fina Technology, Inc., Houston, TX (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 23/00 (2006.01); C08L 23/10 (2006.01); C08L 23/12 (2006.01); C08L 23/16 (2006.01); C08L 9/00 (2006.01);
U.S. Cl.
CPC ...
Abstract

A polymer blend and a method of making the same are provided. The polymer blend includes an ethylene-propylene (C–C) random copolymer and a modifier selected from the group consisting of a metallocene-catalyzed polyethylene-based copolymer, a metallocene-catalyzed polyethylene-based terpolymer, and a syndiotactic polypropylene homopolymer. The polymer blend may also include an organic peroxide for visbreaking the polymer blend. An end use article is made from the foregoing polymer blend. The end use article may be, for example, a film, an injection molded article, a compression molded article, a thermoformed article, and a fiber. The end use article is desirably a film having an Elmendorf tear strength of at least about 300 g/ply in the machine and transverse directions.