The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 17, 2006

Filed:

Aug. 05, 2003
Applicants:

Mitsuru Kato, Okayama, JP;

Kimio Nakayama, Okayama, JP;

Nobuo Takaoka, Okayama, JP;

Inventors:

Mitsuru Kato, Okayama, JP;

Kimio Nakayama, Okayama, JP;

Nobuo Takaoka, Okayama, JP;

Assignee:

Kuraray Co., Ltd., Kurashiki, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08J 3/00 (2006.01); C08K 3/20 (2006.01); C08L 75/00 (2006.01); B32B 5/02 (2006.01); B32B 27/00 (2006.01);
U.S. Cl.
CPC ...
Abstract

Provided are a leather-like sheet fabricated by infiltrating an aqueous resin dispersion (A) into a fibrous substrate, which satisfies a requirement (I) that the aqueous resin dispersion, (A) comprises essentially a main resin (a) stabilized with a surfactant, a polymer (b) having a polyoxyethylene group in its side chains, and a surfactant (c), a requirement (II) that the main resin (a) comprises an urethane resin (a1) and/or an urethane-acrylic composite resin (a2), and the resin skeleton contains from 1 to 10 mmols of a carboxyl group per 100 g of the resin, a requirement (III) that the polymer (b) is obtained through polymerization of a polyoxyethylene group-having ethylenic unsaturated monomer (b1) and any other ethylenic unsaturated monomer (b2) in a ratio by mass (b1)/(b2)=60/40 to 100/0, and a requirement (IV) that the percentage, % by mass (α) of the polyoxyethylene group in the polymer (b) and the number of mols (β) of the amino group per gram of the polymer (b) satisfy 35≦α+β×20000≦60; and an industrial advantageous method for producing the sheet. The leather-like sheet has a good feel and good physical properties.