The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 23, 2006

Filed:

Feb. 09, 2001
Applicants:

Yuichi Itoh, Chiba, JP;

Kunihiko Mizumoto, Chiba, JP;

Hiroyasu Yamaoka, Chiba, JP;

Akira Uchiyama, Chiba, JP;

Inventors:

Yuichi Itoh, Chiba, JP;

Kunihiko Mizumoto, Chiba, JP;

Hiroyasu Yamaoka, Chiba, JP;

Akira Uchiyama, Chiba, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 91/00 (2006.01); C08L 9/00 (2006.01); C08J 3/24 (2006.01);
U.S. Cl.
CPC ...
Abstract

This invention relates to a perfectly or partially crosslinked olefinic thermoplastic elastomer composition which comprises 10 to 90 parts by weight of a crystalline polyolefin (a), 90 to 10 parts by weight of an olefin-based copolymer rubber (b) (the total amount of the components (a) and (b) being 100 parts by weight) and 3 to 100 parts by weight of a paraffinic mineral oil softening agent (c) having an evaporation loss of 0.4% by weight or less at a condition of 200° C., atmospheric pressure and 1 hour and having a kinetic viscosity (40° C.) of 50 to 250 cSt; an olefinic thermoplastic elastomer composition which is obtainable by subjecting a mixture including 40 to 85 parts by weight of an ethylene-based copolymer rubber (A), 60 to 15 parts by weight of an olefinic resin (B) and 45 parts by weight or less of a softening agent (C) [the total amount of the components (A), (B) and (C) being 100 parts by weight] to dynamic heat treatment in the presence of a crossliking agent and which has a gloss value of 80% or more and a haze value of 10% or less on glass plate when subjected to the fogging test at a condition of 100° C. and 3 hours according to the prescription of A method of DIN 75201; and a manufacturing method and use of the compositions.


Find Patent Forward Citations