The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 19, 2005

Filed:

Mar. 04, 1999
Applicants:

Keon-hoon Yoo, Daejeon, KR;

Yang-hyun Shin, Yochon, KR;

Chan-hong Lee, Daejeon, KR;

Inventors:

Keon-Hoon Yoo, Daejeon, KR;

Yang-Hyun Shin, Yochon, KR;

Chan-Hong Lee, Daejeon, KR;

Assignee:

LG Chemical Ltd., Seoul, KR;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C08L009/10 ;
U.S. Cl.
CPC ...
Abstract

Disclosed is a thermoplastic transparent resin composition and a method for manufacturing the same. The resin composition includes 3-15 parts by weight of small aperture polybutadiene rubber latex; 5-25 parts by weight of large aperture polybutadiene rubber latex; 40-70 parts by weight of a methacrylic acid alkylester compound or an acrylic acid alkylester compound; 15-30 parts by weight of an aromatic vinyl compound; and 1-20 parts by weight of a vinylcyan compound. The method includes the steps of a) producing a small aperture polybutadiene rubber latex having an average particle diameter of 600-1500 A, a gel content of 70-95%, and a swelling index of 12-30 by reacting butadiene at 55-70° C. using a polymerization initiator, b) producing a large aperture polybutadiene rubber latex having a particle diameter of 2600-5000 A, a gel content of 70-95%, and a swelling index of 12-30 by enlarging the small aperture polybutadiene rubber latex particles; c) performing graft copolymerization at 65-80° C. by continuously or separately adding 3-15 parts by weight of the small aperture polybutadiene rubber latex of step a), 5-25 parts by weight of the large aperture polybutadiene rubber latex of step b), 40-70 parts by weight of a methacrylic acid alkylester compound or an acrylic acid alkylester compound, 15-30 parts by weight of an aromatic vinyl compound, and 1-20 parts by weight of a vinylcyan compound.