The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 26, 2005

Filed:

Jan. 03, 2003
Applicants:

William Andrew Daunch, Uddingston, GB;

Jan-willem Leenslag, Tremelo, BE;

Hans Godelieve Guido Verbeke, Lubbeek, BE;

Inventors:

William Andrew Daunch, Uddingston, GB;

Jan-Willem Leenslag, Tremelo, BE;

Hans Godelieve Guido Verbeke, Lubbeek, BE;

Assignee:

Huntsman International LLC, Salt Lake City, UT (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08G018/28 ;
U.S. Cl.
CPC ...
Abstract

Process for preparing a flexible polyurethane foam comprising reacting at an isocyanate index of 70 to 130, 1) 40-65 parts by weight of a polyisocyanate composition comprising a) 80-100% by weight of a diphenylmethane diisocyanate component comprising, based on 100 parts by weight of the diphenylmethane diisocyanate component, i) 75-100 parts by weight of diphenylmethane diisocyanate comprising 15-75 parts by weight of 4,4'-diphenylmethane diisocyanate, and 25 to 85 parts by weight of 2,4′-diphenylmethane diisocyanate, and 2,2′-diphenylmethane diisocyanate and/or a liquid variant of such diphenylmethane diisocyanate, and ii) 0 to 25 parts by weight of homologues of diphenylmethane diisocyanates having an isocyanate functionality of 3 or more; and b) 20-0% by weight of toluene diisocyanate; 2) 20 to 45 parts by weight of a polyether polyol having an average molecular weight of 4500-10000, an average nominal functionality of 2-6 and comprising oxypropylene and optionally oxyethylene groups, the amount of oxypropylene groups being at least 70% by weight calculated on the weight of this polyol; 3) 3 to 20 parts by weight of a polyether polyol having an average molecular weight of 700-4000, an average nominal functionality of 2-6 and an hydroxyl value of at most 225 mg KOH/g and comprising oxyethylene and optionally oxypropylene groups, the amount of oxyethylene groups being at least 70% by weight calculated on the weight of this polyol; and 4) 2-6 parts by weight of water, wherein the amount of the polyisocyanate composition, polyol 2), polyol 3), and water being 100 parts by weight.


Find Patent Forward Citations