The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Mar. 15, 2005
Filed:
Mar. 08, 2000
Ryuzo Tomomatsu, Chiba-ken, JP;
Youichi Matsuo, Chiba-ken, JP;
Naoki Narukawa, Chiba-ken, JP;
Tetsushi Yamada, Saitama-ken, JP;
Tetsuya Oda, Saitama-ken, JP;
Ryuzo Tomomatsu, Chiba-ken, JP;
Youichi Matsuo, Chiba-ken, JP;
Naoki Narukawa, Chiba-ken, JP;
Tetsushi Yamada, Saitama-ken, JP;
Tetsuya Oda, Saitama-ken, JP;
Idemitsu Petrochemical Co., Ltd., Tokyo, JP;
Honda Giken Kogyo Kabushiki Kaisha, Tokyo, JP;
Abstract
A propylene-based resin composition has good external appearance due to good weld appearance and low gloss and has excellent mechanical properties such as impact resistance and stiffness. The composition is well-balanced in the external appearance and mechanical properties. Automotive interior trims made of the composition are also described. The propylene-based resin composition comprises (A) 60 to 90% by weight of a propylene-based resin (1) comprising 78 to 88% by weight of 23° C. p-xylene insolubles (a) and 12 to 22% by weight of 23° C. p-xylene solubles (b), (2) the insolubles (a) having an isotactic pentad fraction of 95% or higher, a relaxation time (τ) of 0.01 to 0.35 second at an angular frequency (ω) of 10°/sec when measured by melt viscoelastometry and a molecular weight distribution index (PDI) of 1 to 18 which is expressed by ω/10ωwherein ωis an angular frequency at which a storage modulus (G') as measured by melt viscoelastometry is 2×10Pa and ωis an angular frequency at which a storage modulus (G′) as measured by melt viscoelastometry is 2×10Pa, and (3) the solubles (b) having an intrinsic viscosity [η] (in decalin at 135° C.) of 3.3 dl/g or higher and an ethylene unit content of 43% by weight or smaller; (B) 0 to 10% by weight of a rubberlike elastomer; and (C) 10 to 30% by weight of tale. The automotive interior trims are produced by injection-molding the composition.