The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 08, 2002

Filed:

Feb. 07, 2000
Applicant:
Inventors:

Michael T. K. Ling, Vernon Hills, IL (US);

Lecon Woo, Libertyville, IL (US);

Robert Wojnarowski, Zion, IL (US);

Ketan Shah, Gurnee, IL (US);

Gregg Nebgen, Burlington, WI (US);

Yuan-pang Samuel Ding, Vernon Hills, IL (US);

Varsha Kalyankar, Round Lake Beach, IL (US);

Keith M. K. Anderson, Libertyville, IL (US);

Lillian G. Zakarija, Chicago, IL (US);

Colleen S. Cramer, Racine, WI (US);

Michael Scharf, McHenry, IL (US);

Larry A. Rosenbaum, Gurnee, IL (US);

Assignee:

Baxter International Inc., Deerfield, IL (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 2/708 ; B32B 2/730 ; B32B 2/732 ; B32B 2/734 ; B32B 2/740 ;
U.S. Cl.
CPC ...
B32B 2/708 ; B32B 2/730 ; B32B 2/732 ; B32B 2/734 ; B32B 2/740 ;
Abstract

The present invention provides a multiple layer thermoplastic structure of a (1) skin layer selected from the group consisting of polypropylene, ethylene homopolymers having a density of from about 0.930 g/cc to about 0.960 g/cc, and ethylene homopolymers having a density of from about 0.930 g/cc to about 0.960 g/cc blended with an ethylene and a-olefin copolymers having a density less than about 0.930 g/cc, the skin layer having a thickness of greater than about 3.0 mils; (2) a radio frequency susceptible layer adhered to the skin layer, the radio frequency susceptible layer having a dielectric loss greater than 0.05 at 1-60 MHz and at temperatures of ambient to 250° C., the radio frequency susceptible layer having: (a) a first polyolefin selected from the group consisting of polypropylene and polypropylene copolymers, (b) a second polyolefin selected from the group consisting of ethylene copolymers, ultra-low density polyethylene, polybutene, and butene ethylene copolymers; (c) a radio frequency susceptible polymer selected from the group consisting of (i) ethylene copolymers having 50-85% ethylene content with comonomers selected from a first group consisting of acrylic acid, methacrylic acid, ester derivatives of acrylic acid with alcohols having 1-10 carbons, ester derivatives of methacrylic acid with alcohols having 1-10 carbons, vinyl acetate, and vinyl alcohol (ii) homopolymers and copolymers containing at least one segment of urethanes, esters, ureas, imides, sulfones, and amides, and (d) a compatibilizing agent of a styrene and hydrocarbon copolymer; wherein the structure when fabricated into a 50 ml container has a water vapor transmission rate of less than 8% by weight after the container has been autoclaved at 121° C. for 20 minutes and stored for 90 days in an environmentally regulated compartment having 15% relative humidity at 40° C.