The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Mar. 20, 2001
Filed:
Nov. 22, 1999
Aditi D. Banerjee, Plano, TX (US);
Douglas E. Mercer, Richardson, TX (US);
Rick L. Wise, Plano, TX (US);
Texas Instruments Incorporated, Dallas, TX (US);
Abstract
An embodiment of the instant invention is a method of fabricating an electronic device over a semiconductor substrate, the method comprising the steps of: forming a doped polycrystalline silicon layer insulatively disposed over the semiconductor substrate; and subjecting the doped polycrystalline silicon layer to a temperature of around 700 to 1100 C. in an oxidizing ambient for a period of around 5 to 120 seconds. Preferably, the oxidizing ambient is comprised of: O,,O,, NO, N,O, H,O, and any combination thereof. The temperature is, preferably, around 950 to 1050 C. (more preferably around 1000 C.). The step of subjecting the doped polycrystalline silicon layer to a temperature of around 700 to 1100 C. in an oxidizing ambient for a period of around 5 to 120 seconds, preferably, forms an oxide layer on the polycrystalline silicon layer, which has a thickness which is, preferably, greater than the thickness of a native oxide layer. More preferably, it has a thickness which is greater than 3 nm (more preferably greater than 2 nm). In an alternative embodiment, the thickness of the oxide layer is less than 20 nm (more preferably, less than 10 nm thick).