The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 26, 2000

Filed:

Mar. 01, 1999
Applicant:
Inventors:

Koji Yamamoto, Kanagawa-ken, JP;

Makoto Takahashi, Kanagawa-ken, JP;

Hisashi Shimazaki, Kanagawa-ken, JP;

Katsuya Maruyama, Kanagawa-ken, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08G / ; B32B / ; C08L / ;
U.S. Cl.
CPC ...
528310 ; 528170 ; 528312 ; 528313 ; 528319 ; 528322 ; 528332 ; 528335 ; 528336 ; 428220 ; 4284744 ; 4284745 ; 4284747 ; 4284749 ; 525420 ; 525432 ;
Abstract

A polyamide resin composition comprising 100 parts by weight of a polyamide resin and 0.005 to 1.0 part by weight of at least one compound selected from the group consisting of a metal salt of a fatty acid, a diamide compound and a diester compound. The polyamide resin is obtained by solid phase-polymerizing a polyamide resin prepared by melt-polymerizing a diamine component containing 70 mol % or more of metaxylylenediamine and a dicarboxylic acid component containing 70 mol % or more of adipic acid, and preferably has a relative viscosity of 2.3 to 4.2 when measured at 25.degree. C. using a solution of 1 g polyamide resin in 100 ml of 96% sulfuric acid. By adding at least one compound selected from the group consisting of the specific metal salt of fatty acid, the diamide compound and the diester compound to a solid phase-polymerized polyamide resin, shaped articles such as films, sheets and hollow containers made of the solid phase-polymerized polyamide are improved in the resistance to whitening during storage tinder a high humid condition, upon contacting with water or boiling water, or upon heating to a glass transition temperature or higher.


Find Patent Forward Citations