The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 04, 2000

Filed:

Jul. 16, 1998
Applicant:
Inventor:

Craig Lawrence Sandford, Wheeling, IL (US);

Assignee:

Viskase Corporation, Chicago, IL (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B65B / ;
U.S. Cl.
CPC ...
428 349 ; 428213 ; 428218 ; 428220 ; 428516 ; 264514 ; 264909 ;
Abstract

A multilayer, biaxially stretched, flexible, hermoplastic film having at least three (preferably five) layers (a), (b), and (c) with layer (b) disposed between layers (a) and (c), layers (a) and (c) each being a blend of at least 45% of a copolymer of ethylene and at least one C.sub.3 -C.sub.10 .alpha.-olefin, having a density of 0.900 g/cm.sup.3 to <0.915 g/cm.sup.3, and a melting point between 85.degree. C. and 125 .degree. C. with at least 5% of a high density polyethylene, and layer (b) being at least 45% of a copolymer of ethylene and at least one C.sub.3 -C.sub.10 .alpha.-olefin, having a density of 0.900 g/cm.sup.3 to <0.915 g/cm.sup.3, and a melting point of 85.degree. C.-125.degree. C., the film being 50.8 micrometers(.mu.) or less in thickness, and having a shrinkage value of at least 60% in at least one direction at 127.degree. C., and a process for making the film.