The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 01, 1999

Filed:

Mar. 24, 1998
Applicant:
Inventors:

Thomas Henry Vanderspurt, Delaware Township, NJ (US);

Mark Alan Greaney, Upper Black Eddy, PA (US);

Daniel Paul Leta, Flemington, NJ (US);

Russell John Koveal, Baton Rouge, LA (US);

Mark Michael Disko, High Bridge, NJ (US);

Angela V Klaus, Highland Park, NJ (US);

Sutinder K Behal, Somerville, NJ (US);

Robert B Harris, Billings, MO (US);

Assignee:

Exxon Research and Engineering Co., Florham Park, NJ (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B01J / ; B01J / ;
U.S. Cl.
CPC ...
502349 ; 502324 ; 502340 ; 502343 ;
Abstract

The invention relates to a catalyst for conversion of methanol, ethanol alone or in combination with n-propanol to isobutanol and the process for making and using the catalyst. The catalyst is a noble metal supported on at least a first phase of mixed oxide crystallites containing from about 60 to about 74 atomic % (on a metals basis only) zirconium, from about 21 to about 31 atomic % manganese and from about 5 to about 9 atomic % zinc, and less than about 1 atomic % alkali, a second phase of zirconium-doped hetaerolite particles containing from about 65 to about 69 atomic % manganese, from about 31 to about 35 atomic % zinc, from about 0.5 to about 5 atomic % zirconium, and optionally a trace atomic % of alkali, and a third phase containing from about 29 to about 55 atomic % manganese, from about 13 to about 55 atomic % zinc and from about 13 to about 35 atomic % zirconium. The first phase mixed oxide crystallites have a zirconium oxide-like structure have a particle size of at least about 40 .ANG. to about 100 .ANG., wherein the second phase particles have a particle size of about 200 .ANG. to greater than about 2000 .ANG., and the third phase has a particle size of about 1000 .ANG. to greater than 4000 .ANG..