The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 06, 1999

Filed:

Aug. 23, 1996
Applicant:
Inventors:

Edward L Raymond, Maineville, OH (US);

Robert D Kissinger, Reading, OH (US);

Allen J Paxson, Cincinnati, OH (US);

Eric S Huron, West Chester, OH (US);

Assignee:

General Electric Company, Cincinnati, OH (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C22C / ;
U.S. Cl.
CPC ...
148410 ; 148428 ; 75236 ; 419 11 ;
Abstract

A .gamma.' precipitation strengthened nickel-base superalloy provided in powder metal or cast and wrought form and alloyed to minimize nucleation tendencies and control grain growth. The superalloy includes a fine dispersion of a second phase in sufficient amounts to prevent critical grain growth in the superalloy when the superalloy is subjected to temperatures above its .gamma.' solvus temperature. The superalloy preferably contains at least about 0.030 weight percent carbon or about 27 to about 2000 ppm yttrium in order to produce a volume fraction of the second phase which is sufficient to cover a minimum of about 10 percent of the grain boundary area. The fine dispersion of the second phase restricts the grain boundary motion of the alloy during supersolvus heat treatment, thereby preventing random grain growth during supersolvus heat treatment and yielding a microstructure whose grain size is uniform, for example, having a grain size range of about 2 to about 3 ASTM units and being substantially free of random grain growth in excess of about 2 ASTM units coarser than the desired grain size range.