The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 13, 1998

Filed:

Jun. 03, 1997
Applicant:
Inventors:

Aleksander J Pyzik, Midland, MI (US);

Chan Han, Midland, MI (US);

Uday V Deshmukh, Midland, MI (US);

Kevin J Nilsen, Midland, MI (US);

Donald J Perettie, Midland, MI (US);

Arthur R Prunier, Jr, Midland, MI (US);

Assignee:

The Dow Chemical Company, Midland, MI (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B32B / ; B32B / ; C04B / ;
U.S. Cl.
CPC ...
428 656 ; 428 642 ; 4283202 ; 428328 ; 4285395 ; 4286 / ; 428698 ; 501 87 ; 501 963 ;
Abstract

A hard drive disk substrate is formed of a multi-phase ceramic-based material having at least two phases with amorphous phases being present in an amount less than about 1 volume percent based on the volume of the ceramic-based material or at least one phase being free metal. A process for producing the ceramic-based disk substrate is produced by forming a flat disk of a porous ceramic and then infiltrating the porous ceramic with a metal whereby a multi-phase ceramic-based computer hard drive disk is produced. Additionally, a step of passivating the porous ceramic by elevating it to a temperature of about 1300.degree. to about 1800.degree. C. before the infiltrating step may be performed, such that the surfaces are passivated and the reaction kinetics can be controlled during the infiltrating step. A preferred composite material is made of a multi-phase boron carbide composite material including grains having peaks with an average roughness value, Ra, of between about 1 to about 200.ANG., the roughness value being formed in situ by causing a micro hardness gradient of between about 19 and about 3200 Kg/mm.sup.2 in the various phases of the multi-phase boron carbide composite material.